Comprehensive Study to Understand Longitudinal ERW Seam Failures
Original sourcePDF at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at sourceAttachment at source
Other documents for the same rulemaking
References: 432 extracted, 0 linked to papers
8. Leis, B. N., Brust, F. W., and Scott, P. M., “Development and Validation of a Ductile Flaw Growth Analysis for Gas Transmission Line Pipe,” NG-18-193, 1991(PRCI L51543): see also Brust, F. W. and Leis, B. N., “A New Model for Characterizing Primary Creep Damage,” International Journal of Fracture, Vol 54, pp. 45-63, 1992: see also Brust, F. W. and Leis, B. N., “A Study of Primary Creep Crack Growth At Room Temperatures,” Proc. of the 5th International Conference on Numerical Methods in Fracture Mechanics, ed. A. R.
Luxmoore, and D. R. J. Owen, Freiburg, FRG, pp. 321-332, 1990.
9. Leis, B. N. and Eiber, R. J., “Fracture Control Technology for Transmission Pipelines,” Final Report on PR-003-084506, August 2008: see also Leis, B. N., “Hydrostatic Testing of Transmission Pipelines: When It Is Beneficial and Alternatives When It Is Not”, PRCI Final Report PR 3-9523, 2002. 10. Anon., “API Bulletin on Imperfection Technology,” API Bul. 5T1 (R2010), 2010
11. Leis, B. N. and Nestleroth, J. B., “Battelle’s Experience with ERW and Flash Weld Seam Failures: Causes and Implications,” Interim Final Report on Task 1.4, Contract No. DTPH56-11-T-000003, September 2012.
12. Stonesifer, R. B., Brust, F. W., and Leis, B. N., "Mixed Mode Stress Intensity Factors for Interacting Semi-Elliptical Surface Cracks in a Plate", Engineering Fracture Mechanics, Vol. 45, No. 3, pp. 357-380, 1993.
13. Hahn, G. T., Sarrate, M. and Rosenfield, A.R., “Criteria for Crack Extension in Cylindrical Pressure Vessels”, I J Frac Mech, Vol.5, 1969, pp. 187-210.
14. Hart, B. O., Brongers, M. P. H., Bubenik, T., and Vieth, P. H., “Early Generation Seam Welds,” Final Report R3017-01R, DOT-OPS/PRCI, January 2004. © 2012 Battelle A PPENDIX B - T HE M ODIFIED L N S EC E QUATION AND THE R AJU /N EWMAN E QUATION Kiefner and Associates, Inc. January 2013 Modified LnSec Equation σ −1 − x cos (e )/ (cos −1 (e − y )) σ fs = MP CVN Eπ 12 Equation ML 1 Equation ML 1a CVN Eπ 12 d 0.8 1 − t Equation ML1b 8cσ A 1 1 − M P = o T A
Kiefner, J.F., and Kolovich, K.M., “ERW and Flash Weld Seam Failures” Subtask 1.4 of U.S. Department of Transportation Other Transaction Agreement No. DTPH56-11-T-000003, May 30, 2012.
Kiefner, J.F., Maxey, W.A., Eiber, R.J., and Duffy, A.R., “Failure Stress Levels of Flaws in Pressurized Cylinders”, Progress in Flaw Growth and Fracture Toughness Testing, ASTM STP 536, American Society for Testing and Materials, pp 461 – 481, 1973.
Leis, B. N., Brust, F. W., and Scott, P.M., “Development and Validation of a Ductile Flaw Growth Analysis for Gas Transmission Line Pipe”, Final Report to American Gas Association, NG-18, Catalog No, L51543, 1991.
Anderson, T. L., Merrick, R. D., Yukawa, S., Bray, D. E., Kaley, L., and Van Scyoc, K., “FitnessFor-Service Evaluation Procedures For Operating Pressure Vessels, Tanks, And Piping in Refinery And Chemical Service”, FS-26, Consultants’ Report, MPC Program On Fitness-For-Service, Draft 5, The Materials Properties Council, New York, N.Y., October, 1995.
Harrison, R. P., Loosemore, K., and Milne, I., “Assessment of the Integrity of Structures Containing Defects.” CEGB Report R/H/R6. Central Electricity Generating Board, United Kingdom, 1976.
Jaske, C. E., and Beavers, J. A., “Development and Evaluation of Improved Model for Engineering Critical Assessment of Pipelines”, Proceedings of IPC 2002, 4th International Pipeline Conference, September 29-October 3, 2002, Calgary, Alberta, Canada J.C. Newman, Jr. and I.S. Raju, “An Empirical Stress-Intensity Factor Equation for the Surface Crack”. Engineering Fracture Mechanics, Vol. 15, No. 1-2, pp 185-192, 1981, printed in Great Britain. viii
Eiber, R.J., Hein, G.M., Duffy, A.R., and Atterbury, T.J., “Investigation of the Initiation and Extent of Ductile Pipe Rupture”, Report No. BMI-1793, Progress Report for May-December, 1966, U.S. Atomic Energy Commission Contract No. w-7405-eng-92, January 1, 1967.
Eiber, R.J., Maxey, W.A.., Duffy, A.R., and Atterbury, T.J., “Investigation of the Initiation and Extent of Ductile Pipe Rupture”, Report No. BMI-1866, U.S. Atomic Energy Commission Contract No. w-7405-eng-92, NTIS, July 1969.
Laboratories, ARL 64-174, (October 1964).
Dugdale, D.S., “Yielding in Steel Sheets Containing Slits.”, Journal of the Mechanics and Physics of Solids, Vol. 8, 1960, pp. 100 – 104. Kiefner and Associates, Inc. January 2013
Kiefner, J.F., “Modified equation helps integrity management”, Oil and Gas Journal, Oct 6, 2008, pp 76-82 and “Modified Ln-Secant equation improves failure prediction” Oct 13, 2008, pp 64-66. xiii
Series A, Vol. 221, 1920, pp. 163 – 198. Irwin, G.R., “Analysis of Stresses and Strains near the End of a Crack Traversing a Plate”, Journal of Applied Mechanics, Vol. 24, 1957, pp. 361 – 364.
Barsom, J.M., and Rolfe, S.T., Fracture and Fatigue Control in Structures: Applications of Fracture Mechanics, Third Edition, ASTM Stock Number MNL41, 1999.
Kiefner, J.F., Kolovich, C.E., Zelenak, P.A., and Wahjudi, T., “Estimating Fatigue Life for Pipeline Integrity Management”, IPC04-0167, Proceedings of IPC 2004 International Pipeline
Conference, Calgary, Alberta, Canada (October 4-8, 2004). Kiefner and Associates, Inc. January 2013 Bruce Young and Jennifer O’Brian Battelle Energy Resources September 28, 2016 Teleconference https://primis.phmsa.dot.gov/matrix/PrjHome.rdm?prj=390 The Comprehensive Study to Understand Longitudinal ERW Seam Failures Project Contract No. DTPH56-11-T-000003 Battelle Project No. 100004552 Objective 1. Provide an overview of the project focusing on technical accomplishments used to advance the state of the art in analytical modeling for axial crack-like defects in oil and gas pipeline. 2. Demonstrate the capabilities of PipeAssessTM which implements these analytical models to provide the owners, operators, and regulators advanced, easy-to-use tools to make decisions on safe operation, repair/replace, and re-inspection intervals. Project Review Papers • B. A. Young, S. Nanney, B. L. Leis, and J. M. Smith, “Overview of a Comprehensive Study to Understand Longitudinal ERW Seam Failures” IPC2014-33226,
ASME-IPC 2014, Calgary, Alberta, Canada, September 2014 • B. A. Young, S. Nanney, and J. M. O’Brian, “Review of Phase II for the Comprehensive Study to Understand Longitudinal ERW Seam Failures”, ASME International,
IPC 2016, IPC2016-64142, Calgary, Alberta, Canada, September 2016 Outline • Project Drivers • Phase I Overview • Phase II ▪ Task 1 – Improve Hydrotesting Protocols for ERW/FW Seams ▪ Task 2 – Enhance Defect Detection and Sizing ▪ Task 3 – Defect Characterization: Type, Size, Shape ▪ Task 4 – Model Refinement / V&V • Details of PipeAssessTM (Phase II, Task 5) • Future Concepts • Demonstration of PipeAssessTM Drivers for the Project • Stemmed from the Carmichael, MS rupture in 2007 • NTSB P-09-01 Recommended Comprehensive Study • ERW pipe properties • Assess the means to assure the integrity - so they do not fail in service. • Battelle, KAI, and DNV–Columbus teamed to conduct a comprehensive study to understand longitudinal seam failures in electric resistance welded (ERW) and flash-welded pipes. • Project started in August 2011 • Phase I completed in January 2014 • Phase II completed in August 2017
Phase I, Results • 17 Public Reports in Phase I (https://primis.phmsa.dot.gov/matrix/PrjHome.rdm?prj=390) • 11 Specific Recommendations • Six (6) on Condition Assessment via ILI or Hydrotesting • Three (3) on Predictive Models • One (1) on Local Mechanical and Fracture Properties • One (1) on Aging Pipelines • 2 Presentations: 2014 PRCI Research Exchange Meeting • 5 Presentations: 2014 ASME IPC Outline • Phase II ▪ Task 1 – Improve Hydrotesting Protocols for ERW/FW Seams ▪ Task 2 – Enhance Defect Detection and Sizing ▪ Task 3 – Defect Characterization: Type, Size, Shape ▪ Task 4 – Model Refinement / V&V ▪ Task 5 – Integrity Management Software ▪ Each Task produced a report ▪ Phase II completed in August 2017 Task 1 – Hydrotest Protocols Details can be found in the following paper: R. J. Olson, B. L. Leis, and B. A. Young, “Findings from an Investigation of Hydrotest Protocols”, ASME International, IPC 2016, IPC2016-64146, Calgary, Alberta,
Canada, September 2016 Task 2, ILI & ITDM • 90+ cracks deeper than 25% NWT collected Seam Weld Anomaly (SWA) #1 ➢ Traditional ITDM and IWEX used • Largest cracks installed in Battelle’s Ø16” ILI pull rig ➢ EMAT and transverse MFL used • 19 crack sets identified for validation
DNV Reg. No.: ANEUS811CSEAN120206 Revision No.: 2 Date : November 11, 2012 Page 21
DNV Reg. No.: ANEUS811CSEAN120206 Revision No.: 2 Date : November 11, 2012 Page 22
MANAGING RISK K. Katoh, N. Kosuge, S. Itoh, A. Miyasaka, S. Tanioka, H. Kihira, and T. Murata, Nippon Steel Technical Report, vol. 39/40, p. 15 (1989). T. Hemmingsen, H. Hovdan, P. Sanni, and N.O. Aagones, Electrochimica Acta, vol. 47, p. 3949 (2002). A.G. Howell, "Under-deposit corrosion at weld seams in carbon steel piping", Paper No. 447, Corrosion97, NACE International (1997). R. Wong, Corrosion, in press (2012). J.E. Stead, J. Iron and Steel Institute, vol. 11, p. 5 (1916). T.P. Groeneveld, G.O. Davis, and D.N. Williams, "Evaluations of the susceptibilities of electric-welded pipe to selective seam-weld corrosion", Paper No. 14, Proceedings of Eighth Biennial Joint Technical Peeting on Line Pipe Research, European Pipeline
Research Group, (1991). W.E. Heitmann, P.D. Sothwick, and F. Pausic, "ERW Linepipe: The Effect of Welding and Annealing Upon the Properties, Microstructure, and Corrosion Resistance", p. 957 in International Conferene on Technology and Application of HSLA Steels, ASM International (1984). G. Wranglen, in Sulfide Inclusions in Steel, p. 361, ASM International (1975). Z. Szklarska-Smialowska, Pitting and Crevice Corrosion, NACE International (2005). C.S. Brossia and R.G. Kelly, Corrosion Science, vol. 40, p. 1851 (1998). G. Wranglen, Corrosion Science, vol. 14, p. 331 (1974). P. Sury, Corrosion Science, vol. 16, p. 879 (1976). P. Marcus, J. Chim. Phys., vol. 88, p. 1697 (1991). C.S. Brossia and R.G. Kelly, Corrosion, vol. 54, p. 145 (1998). G.S. Eklund, J. Electrochem. Soc., vol. 121, p. 467 (1974). S.E. Lott and R.C. Alkire, J. Electrochem. Soc., vol. 136, p. 973 (1989). A. Garner, R.J. Brigham, and J.B. Gilmour, "Predicting Localized Corrosion of Weldments with Anodic Dissolution Test", Paper No. 62, Corrosion89, NACE International (1989). L. Tronstad and J. Sejersted, J. Iron and Steel Institute, vol. 127, p. 425 (1933). A. Miyasaka and H. Ogawa, "Grooving Corrosion Behavior of HF-ERW Pipes and Tubes As Influenced By Petroleum Production Environments", Paper No. 26, Corrosion91,
NACE International (1991). C.S. Brossia and G.A. Cragnolino, Corrosion, vol. 56, p. 505 (2000). R. Kiessling, in Non-Metallic Inclusions in Steel, p. 194 The Institute of Metals (1989). A.D. Wilson, Metal Progress, vol. 121, p. 41 (1982). A.D. Wilson, "Clean steel technology - fundamental to the development of high performance steels", in Advances in the Production and Use of Steel with Improved
DNV Reg. No.: ANEUS811CSEAN120206 Revision No.: 2 Date : November 11, 2012 Page 23
MANAGING RISK Internal Cleanliness, ASTM STP1361, J.K. Mahaney, Jr, Editor, ASTM International (1999). G. Krauss, Steels: Heat Treatment and Processing Principles, 2nd ed., ASM International (1990). S. Endo, M. Nagae, S. Fujita, and T. Wada, Welding International, vol. 9, p. 425 (1995). L. Malik, L.D. Parkinson, V. Mitrovic-Scepanovic, and R.J. Brigham, "Effect of weld metal composition on weld zone 1.2%Mn Steel", Proceedings of Intenational Conference of Offshore Mechanics and Arctic Engineering, p. 639, ASME Internatinoal (1990). J. Lee, J. Lee, S. Lim, J. Park, B. Seo, and S. Kim, Corrosion Science and Technology, vol. 31, p. 234 (2002). S. Kusaka, Y. Shinbo, Y. Sekine, S. Kojima, and J. Ohwaki, "Quality of high power laser welded line pipe", Paper No. OMAE98-2752, in 17th International Conference on Offshore Mechanics and Arctic Engineering, ASME International (1998). T.G. Walsh, "Continuous On-Line Weld Corrosion Monitoring for the Oil and Gas Industry", p. 17-1, in International Conference on Pipeline Reliabilty, CANMET (1992). J.F. Kiefner, "Dealing with low-frequency welded ERW pipe and flash welded pipe", Paper No. ETCE2002/PIPE-29029 in ASME Engineering Technology Conference on
Energy, ASME International (2002). M. Baker, "Low Frequency ERW and Lap Welded Longitudinal Seam Evaluation", Integrity Management Program Report DTRS56-02-D-70035, Revision 3, US Department of Transportation, Pipeline and Hanzardous Materials Safety Administration (2004).
DNV Reg. No.: ANEUS811CSEAN120206 Revision No.: 2 Date : November 11, 2012 Page 24
MANAGING RISK APPENDIX - o0o - DNV Reg. No.: ANEUS811CSEAN120106 Revision No.: 2 Date : November 11, 2012 Page M-1 Det Norske Veritas
DNV is an independent organization with dedicated risk professionals in more than 100 countries. Our purpose is to safeguard life, property, and the environment. DNV serves a range of industries, with a special focus on the maritime and energy sectors. Since 1864, DNV has balanced the needs of business and society based on our independence and integrity. Today, we have a global presence with a network of 300 offices in 100 countries, with headquarters in Oslo, Norway. Global Impact for a Safe and Sustainable Future - o0o - Interim Report for Phase II – Task 5 of the Comprehensive Study to Understand Longitudinal ERW Seam Failures “Summary Report for an Integrity Management Software Tool” Authors
Columbus, OH 43201 Prepared for U.S. Department of Transportation Pipeline and Hazardous Materials Safety Administration 1200 New Jersey Ave., SE Washington DC 20590 Contract No. DTPH56-11-T-000003 Battelle Contract No. G006084 Battelle Project No. 100004552 May 2017
Phase II, Task 5 Comprehensive Study to Understand Longitudinal ERW Seam Failures DTPH56-11-T-000003 Battelle does not engage in research for advertising, sales promotion, or endorsement of our clients' interests including raising investment capital or recommending investments decisions, or other publicity purposes, or for any use in litigation. Battelle endeavors at all times to produce work of the highest quality, consistent with our contract commitments. However, because of the research and/or experimental nature of this work the client undertakes the sole responsibility for the consequence of any use or misuse of, or inability to use, any information, apparatus, process or result obtained from Battelle, and Battelle, its employees, officers, or Directors have no legal liability for the accuracy, adequacy, or efficacy thereof. © 2017 Battelle This publication may not be reproduced or distributed without the prior written permission of the copyright owner.
Phase II, Task 5 Comprehensive Study to Understand Longitudinal ERW Seam Failures DTPH56-11-T-000003 Task 2: ILI and ITDM Inspection Assessment Task 3: Defect Characterization: Types, Sizes, Shapes, and Idealizations Task 4: Model Validation Task 5L: Software Development for Integrity Management of Long Seam Welds. This report focuses on the results obtained during the work completed under Phase II, Task 5 which includes the development of a software tool for integrity management. A brief overview of the software will be provided along with Appendices which include the User’s Manual and a presentation made at the 2016 DOT R&D Forum.
Battelle Memorial Institute, 2017. [Online]. Available: http://primis.phmsa.dot.gov/matrix/PrjHome.rdm?prj=390.
[4] B. A. Young, R. Olson and J. O'Brian, "Validation of Fatigue Models for ERW Seam Weld Cracking," in ASME PVP 2017, Waikoloa, 2017.
GEOMETRY: V=v-groove, U=u-groove DIMENSION: 2D=two dimensional analysis model Copyright © 2017 by Battelle Memorial Institute. All Rights Reserved. 17 / 24 PipeAssess PITM User Manual
BS 7910 (2013 & 2015) Note 1 necessary to apply to fatigue Copyright © 2017 by Battelle Memorial Institute. All Rights Reserved. 23 / 24 PipeAssess PITM User Manual Figure 6: Example PipeAssess PI Visualization of Crack Coalesence Software Validation Pending Task 4 Report completion. Works Cited
ASTM International. 2013. E1823-13: Standard Terminology Relating to Fatigue and Fracture Testing. West Conshohocken : s.n., 2013.
Broek, D. 1986. Elementary Engineering Fracture Mechanics. Dordrecht, The Netherlands : Kluwer
Academic Publishers, 1986. Leis, B. N. and Brust, F. W. 1992. NG-18 Report No. 194: Hydrotest Strategies for Gas Transmission Pipelines Based on Ductile-Flaw-Growth Considerations. s.l. : American Gas Association, 1992.
Leis, B. N., Brust, F. W. and Scott, P. M. 1991. NG-18 Report No. 193: Development and Validation of a Ductile Flaw Growth Analysis for Gas Transmission Line Pipe. s.l. : American Gas Association, 1991.
Stonesifer, Randall B, Brust, Frederick W and Leis, Brian N. 1992. Stress-Intensity Factors for Long Axial Outer Surface Cracks in Large R/t Pipes. Philadelphia : Fracture Mechanics: Twenty-Second Symposium (Volume II) , 1992. ASTM STP 1131, pp. 29-45.
Taylor, Craig. 2015. Fatigue Crack Growth of NPS20 Steel Oil Pipe at Varied Orientations. Ontario : University of Windsor, 2015.