Baker and Kiefner Associates Low Frequency ERW and Lap Welded Longitudinal Seam Evaluation TTO Number 5 Apr. 2004
Original sourcePDF at sourceAttachment at source
Other documents for the same rulemaking
References: 21 extracted, 0 linked to papers
OPS TTO5 REV 3.doc April 2004 Michael Baker Jr., Inc.
OPS TTO5 REV 3.doc April 2004 Michael Baker Jr., Inc. Pressure Testing Formats Introduction
API, Recommended Practice for the Pressure Testing of Liquid Petroleum Pipelines, RP 1110, December 1981.
Kiefner, John F., Willard A. Maxey “The Benefits and Limitations of Hydrostatic Testing”, 2000. Page 14
2. Bergman, S. A., “Why Not Higher Operating Pressures for Lines Tested to 90% SMYS?”, Pipeline and Gas Journal, December 1974.
3. Groeneveld, T. P., Davis, G. O., and Williams, D. N., “Evaluations of the Susceptibilities of Electric-Welded Pipe to Selective Seam-Weld Corrosion”, Eighth Biennial Joint Technical Meeting on Line Pipe Research, EPRG/NG-18, May 14-17, 1991.
4. Kiefner, J. F., Maxey, W. A., Eiber, R. J., and Duffy, A. R., “Failure Stress Levels of Flaws in Pressurized Cylinders”, Progress in Flaw Growth and Toughness Testing, ASTM STP 536, American Society for Testing and Materials, pp461-481, 1973.
5. Kiefner, J. F. and Clark, E. B., History of Line Pipe Manufacturing in North America, ASME Research Report CRTD-Vol. 43, Book Number 100396, 292 pages, 1996.
6. Kiefner, J. F. and Maxey, W. A., “Hydrostatic Testing—1, Pressure Ratios Key to Effectiveness”, Oil and Gas Journal, pp 54-61, July 31, 2000.
7. Kiefner, J. F. and Maxey, W. A., “Hydrostatic Testing—Conclusion, Model Helps Prevent Failures”, Oil and Gas Journal, pp 54-58. August 7, 2000. Page 35
8. Kiefner, J. F., “Dealing with Low-Frequency-Welded ERW Pipe and Flash-Welded Pipe with Respect to HCA-Related Integrity Assessments”, Proceedings of Engineering Technology Conference on Energy, Houston, Texas, February 2002.
ILI is an important investigation tool for determining the condition of a pipeline and is a significant part of a pipeline integrity management program recognized by codified provisions that promotes safe, efficient, and cost effective pipeline operation (NACE, 2000). However, all ILI tools are not equally effective for all types of defects. Rather, the selection of the tool, along with its resolution and accuracy requirements, must be targeted to the type of failure mechanism of concern. Code Provisions Relevant to ILI In the proposed rule making for 49 CFR 192, the operator can assess the integrity of a gas pipeline by one of the following methods: 1. Internal inspection (also known as ILI) 2. Pressure testing 3. Direct assessment 4. Any other method that provides an equivalent understanding of the condition of the line pipe 49 CFR 195.452 allows the operator of a liquid pipeline to assess the integrity of the line pipe by the following methods: 1. Internal inspection 2. Pressure testing (in accordance with 49 CFR 195 Subpart E) 3. Any other method that provides an equivalent understanding of the condition of the line pipe of which direct assessment is normally considered an alternative method.
HAZ, and hook cracking (Kiefner, 2002). Hook cracks are manufacturing defects in the longitudinal weld of the pipe, caused by inclusions at the plate edge that are turned out of the plane of the steel during the welding process. It is the turning out of the metal at the weld that gives the characteristic “hook” or “J” shape to the crack (see Figure 5.1). These cracks may pass the manufacturer’s initial hydrostatic test, but fail later due to metal fatigue. Page 38
MFL was the first method fully developed for pipeline ILI and has been the most widely used. (Bickerstaff, and NACE, 2000). The MFL tool induces an axial magnetic flux into the pipe wall between two poles of a magnet. A uniform homogeneous steel pipe without defects creates a uniform distribution of magnetic flux. Metal loss causes a disturbance in the magnetic flux, which, in a magnetically saturated pipe wall, “leaks” out. Sensors detect this leakage caused by the metal loss. Because the measurement of metal loss is indirect, only limited quantification using complex interpretation techniques is possible. MFL can be used to measure metal loss in both gas and liquid pipelines. Based on the testing needs, varying levels of sensitivity can be used. These levels are:
2. Brown, William H., Wilson Rivera, “ILI Data Integratrion: Pipeline Integrity Analysis Using Multiple Inspection Technologies”, 2003.
NACE Corrosion 2002. 4. Kiefner, John F., Willard A. Maxey, “Periodic Hydrostatic Testing Or In-Line Inspection To Prevent Failures From Pressure-Cycle-Induced Fatigue”, 2000 Page 51
Energy, February 2002. 6. NACE Technical Committee Report, “In-Line Nondestructive Inspection Of Pipelines” Publication 35100, December 2000 Page 52
1. ASTM, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products”, A 370, Annual Book of Standards, 2002.
Standards, 2002. 3. Hertzberg, R. W., Deformation and Fracture Mechanics of Engineering Materials, Third Ed., J. Wiley & Sons, Inc., 1989.
ASTM, 1973. 5. Newman, J. C., and Raju, I. S., “An Empirical Stress-Intensity Factor Equation for the Surface Crack”, Eng. Fracture Mechanics, v. 15, Nov. 1981.
6. Rolfe, S. T., and Barson, J. M., Fracture and Fatigue Control in Structures, Prentice-Hall, 1977. Page 78