PHMSA R and D Guidelines for the Identification of SCC Sites and the Estimation of Re-inspection Intervals for SCCDA
Original sourcePDF at sourceAttachment at sourceAttachment at source
Other documents for the same rulemaking
References: 259 extracted, 0 linked to papers
API. 2000. API Recommended Practice 579, Fitness for Service. American Petroleum Institute (Washignton, DC)
ASME. 2004. Managing System Integrity of Gas Pipelines. ASME Code for Pressure Piping, B31. Supplement to ASME B31.8. American Society for Mechanical Wngineers (New
York, NY). Beavers, J.A. and C.L. Durr. 2000. Cathodic protection conditions conducive to SCC. Report prepared for the Corrosion Supervisory Committee, Pipeline Research Council
International, Catalo No. L51897. Beavers, J.A. and R.G. Worthingham. 2002. The influence of soil chemistry on SCC of underground pipelines. Proc. 4th International Pipeline Conference (ASME, New York,
NY), paper IPC2002-27146. Beavers, J.A., C.L. Durr, and B.S. Delanty. 1998. High-pH SCC: temperature and potential dependence for cracking in field environments. Proc. IPC 1998, ASME (New York, NY), Vol. 1, pp. 423-437.
Beavers, J.A., J.T. Johnson, and R.L. Sutherby. 2000. Materials factors influencing the initiation of near-neutral pH SCC on underground pipelines. Proc. International Pipeline
Conf. 2000 (ASME International, New York, NY), vol. 2, pps. 979-988.
CEPA. 2007. Stress Corrosion Cracking. Recommended Practices, 2nd Edition. Canadian Energy Pipeline Association (Calgary, AB).
King, F., T. Jack, M. Kolar, and R. Worthingham. 2004. A permeable coating model for predicting the environment at the pipe surface under CP-compatible coatings. Proc. 5th International Pipeline Conference (ASME, New York, NY), paper IPC04-0368.
NACE. 2008. Stress Corrosion Cracking (SCC) Direct Assessment Methodology. Standard
Practice, SP0204-2008. NACE International (Houston, TX).
NEB. 1996. Stress Corrosion Cracking on Canadian Oil and Gas Pipelines, Report of the
Parkins, R.N. 1994. Overview of intergranular stress corrosion cracking research activities. Report to Line Pipe Research Supervisory Committee of the American Gas Association,
Olive, and R.B. Rebak (eds.), (Elsevier, Amsterdam, 2008), pp. 323-333 Relevant phase(s) in SCC Guidelines: Susceptibility Sub-phase/keywords: Soil type, large-diameter, gas transmission, tape coating, SCC failures, groundwater, pH, redox potential, near-neutral pH SCC, correlation, land use, Russian Results support R&D Guideline no.: Comments: This paper describes Russian experience with developing a “soils model” based on field observations at
Ahmed, T.M., S.B. Lambert, R. Sutherby, and A. Plumtree. 1997. Cyclic crack growth rates of X-60 pipeline steel in a neutral dilute solution. Corrosion 53(7).
Armstrong, R.D. and A.C. Coates. 1976. A correlation between electrochemical parameters and stress corrosion cracking. Corrosion Science 16, 423-433.
Asahi, H., T. Kushida, M. Kimura, H. Fukai, and S. Okano. 1996. The investigation on stress corrosion cracking in a carbonate-bicarbonate solution and its mechanism from metallurgical aspects. Proc. 9th Linepipe Symposium, Pipeline Research Council
Asahi, H., T. Kushida, M. Kimura, H. Fukai, and S. Okano. 1999. Role of microstructures on stress corrosion cracking of pipeline steels in carbonate-bicarbonate solution. Corrosion 55, 644-652.
Asher, S.L. and P.M. Singh. 2009. Role of stress in transgranular stress corrosion cracking of transmission pipelines in near-neutral pH environments. Corrosion 65(2), 79-87.
Atrens, A., Z.F. Wang, N. Kinaev, D.R. Cousens, and J.Q. Wang. 1996. Applicability of ESEM in SCC studies. Proc. 13th Int. Corrosion Congress, Melbourne, Australia, paper no. 233.
Beavers, J.A. 1992. Assessment of the effects of surface preparation and coatings on the susceptibility of line pipe to stress-corrosion cracking. Report to Corrosion Supervisory
Committee, PR186-917, Final Report. Beavers, J.A. 2004. Near-neutral pH SCC: dormancy and re-initiation of stress corrosion cracks. Gas Research Institute Report GRI-7045.
Beavers, J.A. and E.L. Hagerdorn. 1996. Near-neutral pH SCC: mechanical effects on crack propagation. Proc. 9th Linepipe Symposium, Pipeline Research Council International, Catalog No. L51746, paper 24.
Beavers, J.A. and C.E. Jaske. 1998. Near-neutral pH SCC in pipelines: effects of pressure fluctuations on crack propagation. Proc. CORROSION/98, NACE International (Houston, TX), paper no. 257.
Beavers, J.A. and C.L. Durr. 2000. Cathodic protection conditions conducive to SCC. Report prepared for the Corrosion Supervisory Committee, Pipeline Research Council
NY), paper IPC2002-27146. Beavers, J.A. and C.E. Jaske. 2004. Effects of pressure fluctuations on SCC propagation. Pipeline Research Council International Report, Catalog no. L51872e. - A-228 Beavers, J.A. and W.V. Harper. 2004. Stress corrosion cracking prediction model. Proc.
CORROSION/2004, NACE International (Houston, TX), paper no. 04189.
Beavers, J.A., R.N. Parkins, G.H. Koch, and W.E. Berry. 1985. Test method for defining susceptibility of line pipe steels to stress-corrosion cracking. Report to Line Pipe Research Supervisory Committee NG-18, Report No. 146.
Beavers, J.A., W.E. Berry, and R.N. Parkins. 1986. Standard test procedure for stress corrosion cracking threshold stress determination. Corrosion 42, 9-17.
Beavers, J.A., C.L. Durr, and S.S. Shademan. 1998. Mechanistic studies on near-neutral-pH
Beavers, J.A., C.L. Durr, and B.S. Delanty. 1998. High-pH SCC: temperature and potential dependence for cracking in field environments. Proc. IPC 1998, ASME (New York, NY), Vol. 1, pp. 423-437.
Beavers, J.A., C.L. Durr, B.S. Delanty, D.M. Owen, and R.L. Sutherby. 2001. Near-neutral pH
SCC: crack propagation in susceptible soil environments. Proc. CORROSION/2001,
Been, J., F. King, L. Yang, W. Chen, R. Sutherby, and R. Worthingham. 2003. Environmental effects on near-neutral pH SCC. Proc. Northern Area Western Conference, NACE International (Houston, TX), February 3-6, 2003, Calgary, AB, Canada.
Been, J., H. Lu, R. Eadie, G. Shen, and RT. Sutherby. 2004. The role of stress intensifiers in near-neutral pH corrosion fatigue of line pipe. Proc. CORROSION/2004, NACE International (Houston, TX), paper no. 04552.
Been, J., F. King, F. Song, and N. Sridhar. 2004. Coating deterioration as a precursor to SCC. Gas Research Institute Report, GRI-04/0099.
Been, J., L. Yang, H. Lu, and F. King. 2004. Inhibitive effects of organics on near-neutral pH
Been, J., F. King, L. Fenyvesi, and R. Sutherby. 2004. A modeling approach to high pH environmentally assisted cracking. Proc. 5th International Pipeline Conference (ASME, New York, NY), paper IPC04-0361.
Been, J., F. King, L. Yang, F. Song, and N. Sridhar. 2005. The role of coatings in the generation of high- and near-neutral pH environments that promote environmentally assisted cracking. Proc. CORROSION/2005, NACE International (Houston, TX), paper no. 05167. - A-229 Been, J., B. Carroll, A. Dinovitzer, and R. Sutherby. 2006. Stress intensification and crack growth in the presence of dents on pipelines. Proc. IPC 2006, ASME (New York, NY), paper IPC2006-10415.
Been, J., R.R. Fessler, S. Keane, and W. Kresic. 2006. History of pressure fluctuations related to severity of near-neutral pH SCC. Proc. IPC 2006 (ASME, New York, NY), paper IPC2006-10412.
Been, J., R. Eadie, and R. Sutherby. 2006. Prediction of environmentally assisted cracking on gas and liquid pipelines. Proc. 6th International Pipeline Conference (ASME, New York,
NY), paper IPC2006-10345. Been, J., F. King, and R. Sutherby. 2008a. Environmentally assisted cracking of pipeline steels in near-neutral pH environments. Proc. Environmentally Assisted Cracking of Materials. Volume 2: Prediction, Industrial Developments and Evaluation. S.A. Shipilov, R.H.
Jones, J.-M. Olive, and R.B. Rebak (eds.), (Elsevier, Amsterdam, 2008), pp. 221-230.
Been, J., H. Lu, F. King, T. Jack, and R. Sutherby. 2008b. The role of hydrogen in EAC of pipeline steels in near-neutral pH environments. Proc. Environmentally Assisted Cracking of Materials. Volume 2: Prediction, Industrial Developments and Evaluation. S.A. Shipilov, R.H. Jones, J.-M. Olive, and R.B. Rebak (eds.), (Elsevier, Amsterdam, 2008), pp. 255-266.
Blengino, J.M., M. Keddam, J.P. Labbe, and L. Robbiola. 1995. Physico-chemical characterization of corrosion layers formed on iron in a sodium carbonate-bicarbonate containing environment. Corros. Sci. 37, 621-643.
Brongers, M.P.H. and J.A. Beavers. 2005. SCC in areas of local deformation. Gas Research Institute report GRI-04/0127.
Brongers, M.P.H., W. Kovacs, C.S. Scott, and J.A. Beavers. 2009. Stress corrosion cracking in areas of local deformation. Pipeline Research Council International report, Catalog no.
TBD. Brousseau, R. and S. Qian. 1994. Distribution of steady-state cathodic currents underneath a disbonded coating. Corrosion 50 (12), 907-911.
Bueno, A.H.S., B.B. Castri, and J.A.C. Ponciano. 2008. Assessment of stress corrosion cracking and hydrogen embrittlement susceptibility of buried pipeline steels. Proc. Environmentally Assisted Cracking of Materials. Volume 2: Prediction, Industrial Developments and Evaluation. S.A. Shipilov, R.H. Jones, J.-M. Olive, and R.B. Rebak (eds.), (Elsevier, Amsterdam, 2008), pp. 313-322.
Bulger, J. and J. Luo. 2000. Effect of microstructure on near-neutral-pH SCC. Proc. IPC 2000 (ASME, New York, NY), Vol. 2, pp. 947-952.