Policy Replication

L51688B A Modified Criterion for Evaluating the Remaining Strength of Corroded Pipe

Kiefner, Vieth
1989 · report · doi:10.55274/r0011347 · 327 scholarly citations

This paper is behind a paywall; we link to the publisher only.

Cited in 5 places in policy documents

Pipeline Safety: Repair Criteria for Hazardous Liquid and Gas Transmission Pipelines

Federal Register2025-05-21 · DEPARTMENT OF TRANSPORTATION; Pipeline and Hazardous Materials Safety Administration · fn 18
AGA, Pipeline Research Committee Project, PR-3-805, “A Modified Criterion for Evaluating the Remaining Strength of Corroded Pipe” (Dec. 22, 1989)
ailure pressure-based response criterion for any anomalies on their facilities? Would such an approach be more appropriate for some types of anomalies (e.g., metal loss anomalies) than others? And would such a criterion be appropriate for all part 195-regulated hazardous liquid and carbon dioxide pipelines? What amendments to part 192 regulatory language would be necessary when applied to part 195- regulated hazardous liquid and carbon dioxide pipelines? Are the consensus industry standards referenced in part 192 regulations appropriate for calculating predicted failure pressure on hazardous liquid and carbon dioxide pipelines, and what alternatives may be appropriate to consider? \18\ Please provide the technical, safety, and economic reasons for any suggested regulatory amendments, noting in particular the potential compliance costs and implementation challenges associated with adopting a predicted failure pressure-based repair criterion. ---------------------------------------------

Pipeline Safety: Safety of Gas Transmission Pipelines: Repair Criteria, Integrity Management Improvements, Cathodic Protection, Management of Change, and Other Related Amendments

Federal Register2022-08-24 · DEPARTMENT OF TRANSPORTATION; Pipeline and Hazardous Materials Safety Administration · fn 43
AGA, Pipeline Research Committee Project, PR-3-805, "A Modified Criterion for Evaluating the Remaining Strength of Corroded Pipe," (December 22, 1989).
Additionally, these members noted that the proposed criteria for anomalies where corrosion is greater than 50 percent of wall thickness would be redundant with other repair criteria for evaluating corrosion metal loss defects using accepted analysis techniques, such as ASME B31G and remaining strength of corroded pipe (RSTRENG).\43\ Further, for corrosion metal loss affecting pipe seams, members representing the industry suggested the criteria should apply to corrosion that ``preferentially'' affects the long seam,\44\ and that PHMSA should allow an ECA to analyze such defects to prevent unnecessary excavations. --------------------------------------------------------------------------- ---------------------------------------------------------------------------

Pipeline Safety: Safety of Gas Transmission Pipelines: MAOP Reconfirmation, Expansion of Assessment Requirements, and Other Related Amendments

Federal Register2019-10-01 · DEPARTMENT OF TRANSPORTATION; Pipeline and Hazardous Materials Safety Administration · § VI.A
AGA, Pipeline Research Committee Project, PR-3-805, "A Modified Criterion for Evaluating the Remaining Strength of Corroded Pipe," (December 22, 1989).

Pipeline Safety: Pipeline Integrity Management in High Consequence Areas (Gas Transmission Pipelines)

Federal Register2003-01-28 · DEPARTMENT OF TRANSPORTATION; Research and Special Programs Administration · Immediate repair conditions (Section i)
AGA Pipeline Research Committee Project PR-3-805 ("A Modified Criterion for Evaluating the Remaining Strength of Corroded Pipe" (December 1989))

Regulatory Review; Gas Pipeline Safety Standards

Federal Register1996-06-06 · DEPARTMENT OF TRANSPORTATION; Research and Special Programs Administration · Section 192.485 (Remedial Measures: Transmission Lines)
American Gas Association (AGA) report for Project PR 3-805, "A Modified Criterion for Evaluating the Remaining Strength of Corroded Pipe," (December 22, 1989; AGA catalog No. L51609)